Conclusion: Clinically dentin adhesive agents can improve the retentive force and adaption of amalgam restorations.
结论:临床上牙本质粘结剂能改善银汞充填体的固位力和密合度。
Characteristic: Xeno? III Single Step Self etching Dental Adhesive avoids sensitivity by sealing dentinal tubules and eliminating problems of over drying and over - etching of dentin.
特点:异种?三单步自腐蚀牙胶密封避免敏感的牙本质小管和消除问题的干燥和酸蚀牙本质。
Objective: to evaluate the influence of three dentin desensitizers on shear bond strengths of a total-etch adhesive to dentin surfaces.
目的:研究三种牙本质脱敏剂处理牙本质表面后对全酸蚀粘接剂剪切强度的影响。
Influence of Storage Methods on Microtensile Bond Strength of Dentin Adhesive System.
离体牙储存方式对牙本质粘结系统微拉伸强度的影响。
In Group B, the dentin-resin interface of conventionally prepared cavity showed the formation of the hybrid layer, funnel shaped resin tags and adhesive lateral branches.
组传统预备方法的树脂-牙本质界面可见混合层,圆锥型树脂突和侧枝连接的形成;
When bonding the same type dentin substrate, the resin rags were shorter and the hybrid layer thinner in used self-etching adhesive than total-etching adhesive.
全酸蚀粘结系统与自酸蚀粘结系统作用同类型的牙本质上,自酸蚀比全酸蚀形成的混合层薄,树脂突短。
When bonding the same type dentin substrate, the resin rags were shorter and the hybrid layer thinner in used self-etching adhesive than total-etching adhesive.
全酸蚀粘结系统与自酸蚀粘结系统作用同类型的牙本质上,自酸蚀比全酸蚀形成的混合层薄,树脂突短。