• Multiaxial fatigue tests were conducted on 45 steel specimens at room temperature. Thin-walled tubular specimens were subjected to combined tension and torsion loading in low cycle strain control.

    通过多轴疲劳试验,研究了在多轴加载条件下45钢的循环特性变化规律。

    youdao

  • The individual cycle-strain hysteresis loops were recorded, and the cycling response and high temperature low cycle fatigue life were obtained.

    记录了各自的循环应力—应变滞后环,得出了试样的循环响应特征和各试样的高温低周疲劳寿命。

    youdao

  • The individual cycle-strain hysteresis loops were recorded, and the cycling response and high temperature low cycle fatigue life were obtained.

    记录了各自的循环应力—应变滞后环,得出了试样的循环响应特征和各试样的高温低周疲劳寿命。