• Effect degree of regain, relative humidity and test number on breaking tenacity of saw ginned cotton and roller ginned cotton were analyzed respectively through orthogonal test.

    通过正交试验分析了回潮率、相对湿度测试次数三个因素分别对锯齿皮辊棉断裂比强度影响程度

    youdao

  • Test results can be ensured accurate when prolonging adjust-humidity time for saw ginned cotton, increasing test number properly for roller ginned cotton.

    测试锯齿建议延长调湿平衡时间,测试皮辊棉时可适当增加测试次数,以确保测试结果准确

    youdao

  • The correlation between the overlapping number of cotton flock and the process parameters such as effective length of delivery of detaching roller, spun fiber length etc. are discussed.

    探讨了分离罗拉有效输出长度所纺纤维长度参数丛叠合层关系

    youdao

  • This paper analyses and calculates two ranges of standard thickness of the cotton sheet on scutcher, that is, the ranges decided by the process parameter and by the pedal roller evenness regulator.

    分析计算了清机上种棉层标准厚度范围大小,即工艺要求棉层厚度范围天平调节装置允许的棉层厚度范围。

    youdao

  • This paper analyses and calculates two ranges of standard thickness of the cotton sheet on scutcher, that is, the ranges decided by the process parameter and by the pedal roller evenness regulator.

    分析计算了清机上种棉层标准厚度范围大小,即工艺要求棉层厚度范围天平调节装置允许的棉层厚度范围。