The results showed that the lead-free PTC composites which had the size distribution of 30 ~ 70nm could be prepared by citrate sol-gel method.
实验结果表明:利用柠檬酸盐溶胶凝胶法可以合成颗粒粒径在30 ~ 70纳米的无铅ptc陶瓷粉体。
This study adopted the citrate Sol-gel method to prepare the nanophase hexagonal ferrite with doping metal to get high performance microwave materials.
为了获得高性能的微波吸收材料,釆用柠檬酸盐溶胶-凝胶法来制备掺杂有金属离子的纳米六角晶型铁氧体。
The optimum process for preparing nanometer nickel oxide by the citrate-gel method was studied.
优化了柠檬酸盐凝胶法制备纳米氧化镍粉体的工艺条件。
Ferrite-encapsulated cenosphere powders were prepared by citrate sol-gel method. The additive was used to improve the performance of ferrite coating.
研究了柠檬酸盐溶胶-凝胶方法制备空心微珠-钡、锶、钴镍钡铁氧体复合粉体的微观形貌,采用化学添加剂改善铁氧体的包覆性能。
Ferrite-encapsulated cenosphere powders were prepared by citrate sol-gel method. The additive was used to improve the performance of ferrite coating.
研究了柠檬酸盐溶胶-凝胶方法制备空心微珠-钡、锶、钴镍钡铁氧体复合粉体的微观形貌,采用化学添加剂改善铁氧体的包覆性能。