  • The results indicate that the TPV of SBR/BR/LDPE has the exact morphological structure in which the resin is the continuous phase and c

    研究结果证实SBR/BR/LDPE完全硫化共混型热塑性弹性体是以塑料为连续相,交联了的橡胶颗粒为分散相的形态特征。

    youdao

  • The results indicate that the TPV of SBR/BR/LDPE has the exact morphological structure in which the resin is the continuous phase and c

    研究结果证实SBR/BR/LDPE完全硫化共混型热塑性弹性体是以塑料为连续相,交联了的橡胶颗粒为分散相的形态特征。