When bonding temperature was 1403 K, reaction layer grew fast at first and then slow down with the increase of bonding time.
在连接温度为1403K的条件下,随着连接时间的增加,界面反应层厚度先快速增加,再缓慢增加。
The microhardness of the joints increases with increasing of bonding temperature, but it shows a peak value as the bonding time is prolonged.
接头显微硬度随连接温度的升高而明显提高,但随连接时间的变化存在峰值。
Transient liquid phase (TLP) bonding was applied to join TP304H stainless pipe, and the effect of bonding temperature on joint microstructure and mechanical properties was studied.
采用瞬时液相扩散焊(TLP)连接技术进行了TP 304 H不锈钢管的焊接,分析了不同焊接温度对接头组织、成分和力学性能的影响。
Bonding temperature, bonding time and interlayer thickness have an obvious effect on the shear strength of the joints.
连接温度、连接时间和中间层厚度对接头抗剪强度具有较明显的影响。
Bonding temperature, bonding time and interlayer thickness have an obvious effect on the shear strength of the joints.
连接温度、连接时间和中间层厚度对接头抗剪强度具有较明显的影响。