The appropriate bath formulas and deposition conditions for synthesis of Pd-Ni nanowires, in which the percentage of nickle ranging from 8% to 15%, were established.
确定了合成镍含量在8 ~ 15%的钯镍合金纳米线的合适的镀液配方和沉积条件。
Galvanizing bath members effectively protected against the deposition of alloy layers, a process for producing said members, and a method of hot-dip galvanizing that use said members.
有效防止合金层沉积的镀锌槽元件,生产上述元件的方法,和使用该元件的热浸渡方法。
The influence of bath concentrations on deposition rate, composition, surface appearance, formation range of the amorphous structure and corrosion resistance for the deposits was studied.
研究了镀液浓度对镀层沉积速率、成分、表面形貌、非晶态结构形成区域和耐蚀性的影响,得出了最佳镀液浓度及施镀条件。
The influence of bath concentrations on deposition rate, composition, surface appearance, formation range of the amorphous structure and corrosion resistance for the deposits was studied.
研究了镀液浓度对镀层沉积速率、成分、表面形貌、非晶态结构形成区域和耐蚀性的影响,得出了最佳镀液浓度及施镀条件。