结果表明:弹性垫圈断口为典型的沿晶断裂,在断裂的晶面上有细小的爪状纹和微孔。此为高强度钢氢脆断口的特征。
The result shows that it was the typical intergranular fracture, and there were scrappy claw and tiny pore in the fracture of crystal face.
结果表明:弹性垫圈断口为典型的沿晶断裂,在断裂的晶面上有细小的爪状纹和微孔。此为高强度钢氢脆断口的特征。
The result shows that it was the typical intergranular fracture, and there were scrappy claw and tiny pore in the fracture of crystal face.