• 同样晶粒硬度不添加杂质条件下马氏体屈服强度较高冲击断裂以及较低的转变温度,这些都由于较细的平均碳化物尺寸引起。

    For the same grain size and hardness in the unembrittled conditions, martensite has lower yield strength higher Charpy fracture energy and lower FATT due to finer mean carbide size.

    youdao

  • M1M2马氏有着不同的取向结构弹性应变,使得M1和M2不同温度转变氏体

    M1 and M2 are two different martensite variants with diverse elastic strain energy and lattice distortions, which transformation to austenite at different temperatures.

    youdao

  • M1M2马氏有着不同的取向结构弹性应变,使得M1和M2不同温度转变氏体

    M1 and M2 are two different martensite variants with diverse elastic strain energy and lattice distortions, which transformation to austenite at different temperatures.

    youdao