表面碳势为1.1%C的渗碳硬化层内,临近外表面部位的枣核马氏体中会出现显微裂纹。
When carburized under high carbon potential (1. 1% C), microcracks tend to appear on the martensitic matrix near the outer surface of the layer.
表面碳势为1.1%C的渗碳硬化层内,临近外表面部位的枣核马氏体中会出现显微裂纹。
When carburized under high carbon potential (1. 1% C), microcracks tend to appear on the martensitic matrix near the outer surface of the layer.