在一定的实验条件下,除钼、砷、硅的效率均达到95%以上,净化后溶液中杂质含量完全符合技术要求。钨的损失在3%左右。
The Mo, As and Si removed all exceeded 95% of each of their total amounts previously present in the crude solution while the loss of tungsten during the purification amounted to about 3%.
在一定的实验条件下,除钼、砷、硅的效率均达到95%以上,净化后溶液中杂质含量完全符合技术要求。钨的损失在3%左右。
The Mo, As and Si removed all exceeded 95% of each of their total amounts previously present in the crude solution while the loss of tungsten during the purification amounted to about 3%.