• 报导连续波CO2激光加工机对氮化硅陶瓷激光打孔试验,获得了比达18.75的结果

    The test for laser drilling of Si3N4 ceramics by CW CO2 laser processing system is reported. The result shows that the proportion of depth to diameter is 18.75.

    youdao

  • 报导连续波CO2激光加工机对氮化硅陶瓷激光打孔试验,获得了比达18.75的结果

    The test for laser drilling of Si3N4 ceramics by CW CO2 laser processing system is reported. The result shows that the proportion of depth to diameter is 18.75.