    When the heating rate was fast enough, the iron joined crystal could be formed.

    youdao

  • 介绍了影响碳钢工艺操作和设备。

    The possibility of transverse corner cracking in slab of peritectic carbon steel is greater than that of other carbon steels.

    youdao

  • 降低钢水浇注过热度提高等轴有效措施。

    Low superheat casting is the important method of increasing equiaxed crystal ratio of bloom.

    youdao

  • 发明属于偏合金技术,具体地说是一种偏型合金薄板方法。

    The present invention relates to continuous casting technology of monotectic alloy, and is especially continuous casting process of monotectic alloy sheet.

    youdao

  • 通过确定凝固速度表达式定量计算过程中一次间距

    Based on the conformation of the solidification rate expression, the quantitative calculation of the primary dendritic spacing in the continuous casting was done.

    youdao

  • 通过确定凝固速度表达式定量计算过程中一次间距

    Based on the conformation of the solidification rate expression, the quantitative calculation of the primary dendritic spacing in the continuous casting was done.