  • 硫酸废热锅炉故障主要受热面管子磨损受热面腐蚀过热爆管焊缝漏水等引起的。

    Abrasion and corrosion of heating surface, superheater tube cracking and weld leakage are the main cause of waste heat boiler breakdown in sulphuric acid plant.