用乳化浸渍的方法,由交联聚丙烯酸、聚丙烯酸甲酯、氢氧化钾和水制备了准固态复合聚合物电解质(QSPE)膜。
Composite quasi solid polymer electrolyte(QSPE) membrane composed of cross-linked polyacrylic acid, polymethyl acrylate, KOH and H_2O was prepared by emulsification and soaking process.
通过紫外光引发甲基丙烯酸甲酯的接枝聚合,在聚丙烯膜表面引入了反应性基团酯基。
The surface of polypropylene microporous membranes was activated by the graft polymerization of methyl methacrylate initiated with ultraviolet-photo.
以丙烯酸、 丙烯酸丁酯和甲基丙烯酸甲酯为单体,采用自由基聚合法制备了聚丙烯酸卷材涂料前驱成膜物,获得了适宜的制备工艺条件。
Phragmoplast of coil coating has been prepared by free radical polymerization and by using acrylic acid, methyl methacrylate, butyl acrylate as the raw materials.
以丙烯酸、 丙烯酸丁酯和甲基丙烯酸甲酯为单体,采用自由基聚合法制备了聚丙烯酸卷材涂料前驱成膜物,获得了适宜的制备工艺条件。
Phragmoplast of coil coating has been prepared by free radical polymerization and by using acrylic acid, methyl methacrylate, butyl acrylate as the raw materials.