在浸没循环撞击流反应器中,以硝酸钙和磷酸钠为原料、乙酰胺为分散剂,采用水热法合成了纳米羟基磷灰石。
Nano - hydroxyapatite was synthesized by hydrothermal method in the submerged circulating impinging stream reactor, using calcium nitrate and sodium phosphate as reactants and acetamide as dispersant.
HA具有羟基、羧基和乙酰胺基等官能团,可通过交联、酯化、接枝、分子修饰和复合等方法进行改性。
Ha has functional groups such as hydroxyl, carboxyl and N-acetyl, therefore, it can be modified by cross-linking, esterification, graft, molecule modification and composition.
以对羟基苯乙酰胺为原料,经烷基化、水解、酯化、氧肟化等4步反应合成丁苯羟酸,总收率为46.5%。
With pHydroxybenzeneactamide as the starting material, the Bufemaxac was prepared by means of four steps reaction of alkylation, hydrolyzing, esterification and Ooximation with total yield of 46.5%.
以对羟基苯乙酰胺为原料,经烷基化、水解、酯化、氧肟化等4步反应合成丁苯羟酸,总收率为46.5%。
With pHydroxybenzeneactamide as the starting material, the Bufemaxac was prepared by means of four steps reaction of alkylation, hydrolyzing, esterification and Ooximation with total yield of 46.5%.