本研究详细考察了微细拉黑钨矿剪切絮凝浮选的主要影响因素。
In this paper, the effect of various main factor on the shear-flocculation flotation of ultrafine wolframite particles was investigated.
近年来研究开发的褐铁矿选矿技术主要包括:重选、磁选等单一流程和选择性絮凝浮选等联合流程。
Beneficiation techniques on limonite developed in recent years mainly include single process of gravity or magnetic separation etc. and combined processes with selective flocculation flotation etc.
对含油污水过滤、隔油、浮选、絮凝和应用油水分离器等具体处理方法。
Detailed methods including filtration, separation, floatation, flocculation and use of oil and water separator are also recommended.
絮凝脱泥-反浮选流程适应东鞍山难选矿石特性。
The flocculation desliming-reverse flotation flowsheet is compatible with the characteristics of Donganshan refractory iron ore.
本发明涉及采用浮选的水处理设备,其至少包括:待处理水的入口区(31),所述待处理水预先进行凝聚和絮凝;
The invention relates to a flotation water treatment plant comprising at least: an inlet zone (31) for the water to be treated, which is coagulated and flocculated beforehand;
结果表明,采用选择性絮凝脱泥-阳离子反浮选流程闭路试验可获得铁精矿品位为65.50%,回收率为83.09%的较好指标。
The results showed that, an iron concentrate with a TFe grade of 65.50% and a recovery of 83.09% can be obtained by the closed-circuit bench test.
结果表明,采用选择性絮凝脱泥-阳离子反浮选流程闭路试验可获得铁精矿品位为65.50%,回收率为83.09%的较好指标。
The results showed that, an iron concentrate with a TFe grade of 65.50% and a recovery of 83.09% can be obtained by the closed-circuit bench test.