目的:初步研制纳米复合磷酸锌水门汀。
结论磷酸锌水门汀基是防治内漂白后牙颈部外吸收的一种有效方法。
Conclusion The zine oxide phosphorate base was a kind of effective measure to prevent post-bleaching external cervical resorption.
探讨并记录护髓垫底材料玻璃离子粘固剂与自凝氢氧化钙联合磷酸锌水门汀治疗后牙深龋的疗效并进行比较。
Explored and recorded the curative effect of protecting pulp bottom material glass ion curing agent and self-congealing hl joint zinc phosphate cement posterior teeth with deep caries repaired.
结果:两种封闭介质对种植体表面应力分布的影响没有显著性差别,但玻璃离子水门汀的抗折性优于磷酸锌水门汀。
Results:For zinc phosphate and glass-ionomer, similar Von Mises stress was found in each part of the implant, but glass-ionomer had the better ability of resistance to fatigue than zinc phos…
不同粘接剂对桩的固位力大小有显著性影响,树脂粘接剂的粘接强度为玻璃离子和磷酸锌水门汀的1.5 - 2.0倍。
Resin cements have been reported to produce 150% to 200% the retention strength of zinc phosphate and glass ionomer cements.
不同粘接剂对桩的固位力大小有显著性影响,树脂粘接剂的粘接强度为玻璃离子和磷酸锌水门汀的1.5 - 2.0倍。
Resin cements have been reported to produce 150% to 200% the retention strength of zinc phosphate and glass ionomer cements.