• 试验结果表明加入湿法白炭黑试样拉伸强度比添加气相法白炭黑者提高了54%,扯伸长提高了64%,磨耗降低20%。

    The results showed that the sample by adding the ultrafine powders of silica aerogel increased the tensile strength 54%, the elongation at break 64%, decreased the abrasion loss 20%.

    youdao

  • 试验结果表明加入湿法白炭黑试样拉伸强度比添加气相法白炭黑者提高了54%,扯伸长提高了64%,磨耗降低20%。

    The results showed that the sample by adding the ultrafine powders of silica aerogel increased the tensile strength 54%, the elongation at break 64%, decreased the abrasion loss 20%.