实验还表明,单丝的拉伸强度和相对伸长率与它的加工温度、形态和熔化程度有密切的关系。
The experiment shows that the tensile strength and elongation of monofilament depend largely on the processing temperature, morphology and fusion level.
相对于常规奥氏体轧制,铁素体轧制薄板的屈服强度下降了20%左右,伸长率及应变硬化指数与之相当。
Compared with the strip produced by conventional austenite rolling, the yield strength of the ferrite rolled strip was lower by about 20%, with same elongation and strain hardening exponent.
高固含量PIPA多元醇泡沫相对于POP多元醇泡沫,具有更好的压陷硬度、回弹率、 拉伸强度、 伸长率以及撕裂强度等机械性能。
Relative to the foam added with POP polyol, the foam added with high solid content PIPA polyol has the better mechanical performance on the resilience coeffi…
高固含量PIPA多元醇泡沫相对于POP多元醇泡沫,具有更好的压陷硬度、回弹率、 拉伸强度、 伸长率以及撕裂强度等机械性能。
Relative to the foam added with POP polyol, the foam added with high solid content PIPA polyol has the better mechanical performance on the resilience coeffi…