研究了药芯焊丝在CO2保护电弧堆焊过程中合金元素的过渡系数。
The transition coefficients of alloying from cored wire to deposited metal during CO2 GMAW have been studied in this paper.
其综合作用使碳极氩气拘束电弧堆焊稀释率低,合金元素过渡系数高。
The synthesis results are that the dilution rate of surfacing of carbon electrode arc constrained by argon is low and the transfer coefficient of alloy elements is high.
试验研究了碳化钨耐磨药芯焊丝电弧堆焊工艺方法对堆焊层性能和组织的影响。
The influence of arc surfacing method on the property and structure of the surfacing layers were studied.
采用堆焊焊条CHR322,在A 3钢基体上以不同的焊接工艺进行手工电弧堆焊试验。
Surfacing process is conducted on the substrate of steel A3 by shielded metal arc welding process using electrode CHR322 under different welding current conditions.
前言:采用焊条电弧焊工艺方法,选用C HR322堆焊焊条在Q235钢基体上以不同的焊接电流进行了堆焊试验。
Surfacing process test is made on Q235 steel substrate by shielded metal arc welding process using electrode CHR322 at different welding current condition.
采用平板堆焊的方法及高速摄像系统,研究了双电极钛钙型碳钢焊条的焊芯间距对焊接工艺和电弧形态的影响。
The effect of span between two cores of lime-titania type carbon-steel electrode was investigated using the method of overlay welding on the plate work-piece and high speed camera system.
借助手工电弧焊方法,使用CHR系列堆焊焊条对A 3、45钢进行堆焊加工,分析了其堆焊层金属的显微组织及性能。
With SMAW method, the surfaces of A3 and 45 steel were welded by using the series of CHR electrode, and the microstructure and performance of surfacing welding layer metal were analyzed.
借助手工电弧焊方法,使用CHR系列堆焊焊条对A 3、45钢进行堆焊加工,分析了其堆焊层金属的显微组织及性能。
With SMAW method, the surfaces of A3 and 45 steel were welded by using the series of CHR electrode, and the microstructure and performance of surfacing welding layer metal were analyzed.
应用推荐