羰基镍粉可形成受控制的高空隙烧结电极。
T255 type carbonyl nickel powder can form controllable high-rate gap baking electrode.
自焙电极是大型制磷电炉的关键技术之一,单位产品的电极消耗费用比预烧结电极的低得多。
Soderberg electrode is the one of the critical technologies for large-scaled electric phosphorus furnace. The electrode consumption of unit product is much lower than that of pre-sintering electrode.
介绍了铜钨粉末烧结材料的性能特点,以及用此材料制成的电极和导电咀在焊按生产中的使用效果。
The performance features of copper-tungsten sintered materials and operating effects of electrode and nozzle made of the materials in welding production have been introduced.
同时,铝浆厚膜烧结层又作为背面电极。
Simultaneously, the SP aluminum thick film layer is the rear electrode.
结果表明,随着烧结温度的增加,镍电极附着力逐渐增大, 方阻逐渐下降;
With the increase of the sintering temperature, the adhesion force of Ni electrodes enhances, and the square resistance decreases.
提出了PTC消磁热敏电阻器生产过程中的几个关键质量控制点,主要包括原料控制、造粒压片控制、烧结工艺控制、电极控制等四方面。
The key quality control points in PTC degaussing thermistor production are presented, including the control over raw material, granulation and press, firing and electrode process.
我们曾经报告过利用铝电极和锡或锡合金探头之间的烧结现象来实现接触的过程。
We report on the contact process utilizing fritting phenomena between al electrode and probes made of tin or tin gold alloy.
钛酸锌微波介质陶瓷因其优异的介电性能、较低的烧结温度,而被广泛应用于制备银、铜电极共烧中温低介微波材料中。
As ZnTiO3 has the outstanding dielectric property and low sintering temperature, it has been mixed with Ag, Cu, etc. to prepare electrodes at relatively low sintering temperature.
本系列银浆为外部电极可焊银浆,广泛应用电子陶瓷元件,烧结后具有良好的焊接适应性。
The silver paste series is external electrode solderable silver paste, widely applied to electronic ceramic parts, which has good welding adaptability after.
最后分层蒸镀、烧结制备电极,去边处理后完成电池片的制备。
Finally, evaporate and sinter layers to form electrode, trim the edge of the chip to complete the battery manufacture.
研制结果表明国内烧结良好的陶瓷介质完全可以制成镍电极陶瓷电容器,投入工业生产。
The result of the development shows that properly sintered ceramic dielectric is good enough to be employed for…
不适当的烧结温度和保温时间都会造成各种缺陷,甚至电极变形毁坏,造成电极电化学性能下降。
Inap- proriate sintering temperature and holding time will make a variety of defects, even destruct the electrode, cut down the performance.
不适当的烧结温度和保温时间都会造成各种缺陷,甚至电极变形毁坏,造成电极电化学性能下降。
Inap- proriate sintering temperature and holding time will make a variety of defects, even destruct the electrode, cut down the performance.
应用推荐