与经普通淬火和高温回火的相比,经磁场淬火和高温回火的T10钢的抗拉强度提高了28%,断后伸长率提高了8。
The tensile strength, elongation and hardness of T10 steel subjected to magnetic field quenching and to high temperature tempering were separately increased by 28%, by 8.
以一个全封闭恒温车间内热处理油烟的收集与净化为例,介绍了井式淬火油槽和井式回火炉中所产生油烟的收集与净化方法。
A method for gathering and purifying the oil smoke which was produced by oil quenching tanks and tempering in the whole-sealed and constant-temperature heat treatment plant was introduced.
无论是淬火或淬回火态的试样其热疲劳裂纹主要沿着碳化物与基体脱开处及晶界裂纹桥接而扩展。
The thermal fatigue crack propagated mainly through the break-age of the interface of carbide and grain boundaries for either quenched or quenched and tempered steel.
探讨了淬火及回火热处理对激冷铸铁白口层的显微组织与耐磨性的影响。
The influences of quench and temper treatment on the microstructure and wear resistance of white layer of the chilled cast iron were discussed.
探讨了淬火及回火热处理对激冷铸铁白口层的显微组织与耐磨性的影响。
The influences of quench and temper treatment on the microstructure and wear resistance of white layer of the chilled cast iron were discussed.