• 无水提塔喷嘴高速蒸汽产生介质活化腐蚀作用腐蚀严重通过材质、结构优化取得良好的效果。

    By the joint action of cavitation corrosion produced in the high speed stream and medium activation corrosion, the spray nozzles of anhydrous ammonia stripper corrode seriously.

    youdao

  • 无水提塔喷嘴高速蒸汽产生介质活化腐蚀作用腐蚀严重通过材质、结构优化取得良好的效果。

    By the joint action of cavitation corrosion produced in the high speed stream and medium activation corrosion, the spray nozzles of anhydrous ammonia stripper corrode seriously.