平板工件中心存在较大的残余应力分布区。
High residual stress distribution zone lies in the center of work piece.
根据磁畴壁运动唯象理论,得到残余应力分布曲线。
The distribution curves of residual stress for these samples were obtained based on the phenomenon theory of wall motion.
实测了激光相变硬化区的宽度和深度及残余应力分布。
The width and depth of laser transformation hardening zone and residual stress distribution were measured experimentally.
渗层中的相变次序和残余奥氏体的存在对残余应力分布影响较大。
Phase transformation sequence in diffusion layer and the existence of residual austenite have great effect on the distribution of residual stress.
残余应力分布状态及表面租糙度是评定加工表面层质量的两个重要参数。
Residual stress profile state and surface roughness are the two important parameters for evaluating machined surface layer quality.
金属焊接引起的残余应力分布的不均匀程度是影响设备寿命的重要因素。
Weld residual stress degree of irregularity is the important influencing factor for equipment life.
本文对激光冲击成形的3a 21防锈铝板的残余应力分布特性进行了研究。
Distributing characteristics of the residual stress of 3a21 antirust aluminum by laser shock processing are studied.
利用弹塑性理论建立了孔冷挤压的载荷、位移、应力以及残余应力分布表达式;
The expressions of load, displacement, stress and residual stress distribution for hole cold_extrusion process are established by using elastic_plastic theory.
采用有限元分析法和X射线应力测试法对铍环形焊件的残余应力分布规律进行了研究。
The residual stress of the beryllium ring weldment was studied by FEM simulation and X ray stress measurement.
计算了成形后交叉缩放椭圆管的残余应力分布并比较了三个典型截面上的残余应力状况。
The three-dimensional distribution of residual stress was investigated and the residual stresses on three representative sections were compared.
简要阐明了造成不同焊缝应力分布的原因及火工校弯成形工艺对构件残余应力分布的影响。
The reasons for different mode of welding residual stress distribution and influence of flame curving on steel structure are discussed.
中子衍射方法可以用来测量材料内部的三维残余应力分布,是一种重要的无损检测分析手段。
Neutron diffraction, an important non-destructive testing method, can facilitate 3-d mapping of residual stress in a bulk component.
利用X射线无损检测方法,对铸造铝合金制造的某发动机汽缸体的残余应力分布进行了全面分析。
Residual stress distribution for engine cylinder body made of casting aluminum alloy was investigated completely using X-Ray nondestructive detection method.
借助现代冶金分析技术对闭塞冷锻行星齿轮的晶粒尺寸、硬度变化和残余应力分布规律进行了研究。
By virtue of modern metallograph analyse technology, the size of grain, hardness and residual stress of bevel gear by closed-die cold forging is studied.
本文就冷胀孔周残余应力分布的测量技术和干涉螺接孔周干涉应力分布的测量技术进行了实验研究。
An experimental study was conducted to measure residual stress distribution around cold-expanded fastener holes and interference stress distribution near interference fit fastener holes.
借助现代冶金分析技术对闭塞冷锻行星齿轮的晶粒尺寸、硬度变化和残余应力分布规律进行了研究。
The numerical simulation method was applied to analyze the cold closed-die forging process of car used differential satellite gear.
借助现代冶金分析技术对闭塞冷锻行星齿轮的晶粒尺寸、硬度变化和残余应力分布规律进行了研究。
Study on microstructure and properties of closed-die cold forging of bevel gear used in case of automobile differential;
结果表明,装夹位置对残余应力分布具有重要影响,而装夹顺序对残余应力的分布和幅值无较大影响。
It is verified that clamping points have great effect on the residual stress, but that of the clamping order is little.
冷弯薄壁型钢截面上的残余应力分布是弯曲型的,而热扎型钢或焊接型钢截面上残余应力分布是薄膜型。
Cold-formed steel cross section on the residual stress distribution is curved, and hot rolling steel or steel section on welding residual stress distribution is a thin film type.
研究了焊接贝氏体-奥氏体钢管贝氏体钢侧显微组织变化和残余应力分布对巴克豪森噪声(BN)的影响。
The effects of change in microstructure and residual stress distribution on Barkhausen noise (BN) on the bainitic steel side in a welded bainitic and austenitic steel pipe are studied.
在铣削加工零件时,零件各部分的残余应力分布不均匀,会使工件发生变形,影响工件的形状和尺寸精度。
In the milling procedure, the distribution of stress inside material is uneven, which makes the work-piece deformed and affects shape and dimension precision.
焊缝氢含量的测试分析表明,阵列式射流冲击热沉系统可以改善接头的残余应力分布,防止冷却水侵入焊缝。
The hydrogen contents investigations show that the FSW process with array jet impingement sink appaatus can prevent the joints form the effect of colding water.
受厚板截面本身的几何形状所影响,箱形截面有焊缝一侧壁板与另一侧壁板残余应力分布及大小有明显的不同。
Affected by the geometry of box-section, the residual stress distribution of plate with welding passes is different from that of another plate.
用x2350a型x射线应力衍射仪测试冲击区域残余应力分布情况,并用有限元软件ABAQUS进行模拟。
X2350A X-ray strain instrument was introduced to test the residual stress in the shocked region, and finite element software ABAQUS was used to simulate the stress.
为了有效检测铝合金材料上的残余应力分布,研究了用激光超声技术来检测铝合金材料上的残余应力分布的方法。
In order to effectively determine the residual-stress profile of an aluminum alloy, the measuring method was studied by the laser ultrasonic technique.
针对7075铝合金中厚板真空电子束焊接过程,采用非线性有限元法,对焊接接头的残余应力分布进行了数值模拟。
Aim at 7075 aluminium alloy vacuum electronic beam welding, using nonlinear finite element, the numerical simulation of the residual stresses distribution in welding joint was made.
将计算得到的残余应力分布与实测的残余应力数据进行比较,两者符合较好,而且高温回火有效的降低了焊接残余应力的峰值。
Compared the welding residual stress with testing data, the both accord each other, and high temperature temper reduce the peak value of welding residual stress effectively.
结果表明:在役焊接接头残余应力分布规律与常规焊接保持一致,符合管道焊接接头“内凸外凹”的变形机理,但在数值上差别较大。
Results show that distribution regularity of residual stress of in-service keeps coherent with routine welding, which measures up deformation mechanism of welding, but numeric value is different.
结果表明:在役焊接接头残余应力分布规律与常规焊接保持一致,符合管道焊接接头“内凸外凹”的变形机理,但在数值上差别较大。
Results show that distribution regularity of residual stress of in-service keeps coherent with routine welding, which measures up deformation mechanism of welding, but numeric value is different.