分析结果表明,铸锭中分布不均匀的非金属夹杂物和组织中过量分布于晶界的贝氏体和三次渗碳体是导致冷镦开裂的原因。
It was revealed that: inhomogeneous distribution of the non-metallic inclusion and excessive bainite and tertiary cementite is the cause of cracking.
以上诸因素的共同作用,使贝氏体具有比直接淬火所获得的马氏体更高的二次硬化效应、热强性和组织稳定性。
As a result of the coaction of abovementioned factors, the bainite has superior secondary hardening effect, thermal strength and structural stability to martensite formed by straight tempering.
以上诸因素的共同作用,使贝氏体具有比直接淬火所获得的马氏体更高的二次硬化效应、热强性和组织稳定性。
As a result of the coaction of abovementioned factors, the bainite has superior secondary hardening effect, thermal strength and structural stability to martensite formed by straight tempering.