• 传统树脂转注成型成型时间约为60分钟一个循环但是CMC成型时间依不同厚度要求只需3-7分钟。

    Typical cycle times run 60 minutes up per part via RTM. However, the cycle time of CMC is only 3-7 minutes depending on the thickness of the sheet.

    youdao

  • 传统的浸布树脂转注成型来说避免树脂过多,或是树脂缺乏区域,甚至在成品性能妥协一件困难的事。

    It would be difficult with complex shape to use prepreg mat or RTM process without having resin-starved or resin-rich area, compromising performance.

    youdao

  • 传统的浸布树脂转注成型来说避免树脂过多,或是树脂缺乏区域,甚至在成品性能妥协一件困难的事。

    It would be difficult with complex shape to use prepreg mat or RTM process without having resin-starved or resin-rich area, compromising performance.