采用硫酸镍、钨酸钠和柠檬酸三钠为基本组分的镀液,通过电镀的方法在紫铜试片上沉积得到了镍钨合金镀层。
Nickeltungsten alloy coating was deposited on copper plate making use of electroplating in the bath composed of nickel sulfate, sodium tungstate, and trisodium citrate.
采用硫酸镍、钨酸钠和柠檬酸三钠为基本组分的镀液,通过电镀的方法在紫铜试片上沉积得到了镍钨合金镀层。
Nickeltungsten alloy coating was deposited on copper plate making use of electroplating in the bath composed of nickel sulfate, sodium tungstate, and trisodium citrate.