• 结果表明溶胶结合减少了粉扩散体积收缩得到不锈钢结合良好开裂涂层

    The results show that the combination of ZrO2 gel and nano-powder decreases diffuse and volume shrinkage. The coating which has no crack and good combination with stainless steel is obtained.