结果表明,在热湿条件下老化结束后,材料的断裂应力、初始模量和断裂比功的损失率分别大于44%、65%和51%;
The results showed the loss rates of stress, initial modulus and breaking work were more than 44%, 65% and 51% after hydrothermal aging test respectively;
结果表明,在热湿条件下老化结束后,材料的断裂应力、初始模量和断裂比功的损失率分别大于44%、65%和51%;
The results showed the loss rates of stress, initial modulus and breaking work were more than 44%, 65% and 51% after hydrothermal aging test respectively;