介绍了涂膜拉伸强度、断裂时的延伸率,防碳化效应特性试验以及弹性外墙乳胶涂料施工应用技术。
Tests on film tension strength, elongation rate at breaking, anti carbonation effect etc. and applied technique of elastomeric latex coating for exterior wall are described.
合金在高应变速率的变形中通过动态再结晶可获得更细的晶粒尺寸,其断裂时总延伸率在135%左右。
They also show that a finer grain size can be obtained by dynamic recrystallization during superplastic deformation at a high strain rate, but the total elongation to failure is limited in about 135%.
不同电位下,SRB存在时试样的断裂延伸率均低于海泥中不含SRB时的断裂延伸率。
The elongation rates of the specimens in marine mud with SRB under different potentials are lower than those in marine mud without SRB.
不同电位下,SRB存在时试样的断裂延伸率均低于海泥中不含SRB时的断裂延伸率。
The elongation rates of the specimens in marine mud with SRB under different potentials are lower than those in marine mud without SRB.