介绍了一种自行设计的夏比冲击试验V形缺口试样送样卡具。
This article introduced a kind of self-designed V shape sample clamp for Sharpy impact test machine.
通过不同温度条件下不同厚度、不同缺口取向含V形缺口试样进行3点弯曲试验研究,发现X70管线钢具有严重的各向异性现象,其在平行钢板表面方向和沿钢板厚度方向力学性能差异较大。
The effects of thickness and notch orientation on the toughness of X70 pipeline steel samples with V notch were investigated experimentally by use of the 3-point bending test at different temperature.
缺口试样在缺口的高应力集中效应下,加快疲劳裂纹形核过程。
The high stress concentration effect of notch can accelerate the process of fatigue crack nucleation in the notch specimen.
缺口试样在缺口的高应力集中效应下,加快疲劳裂纹形核过程。
The high stress concentration effect of notch can accelerate the process of fatigue crack nucleation in the notch specimen.