用基于风险检验评估方法分析了石化装置中运行的高温设备发生脆性断裂失效的可能性,介绍了利用回火脆化损伤因子确定最低升压温度的计算方法,为装置安全生产提供了可靠依据。
The method to determine the minimum upset temperature by means of the damage factor of temper embrittlement was introduced, and the dependable basis for equipment safe operation was offered.
在试验的焊接条件下,WCX355超细晶钢在热影响粗晶区未有明显脆化,在回火区也未发生软化现象。
Under the experiment's welding condition, WCX355 ultrafine grained steels didn't distinctly embrittle in CGHAZ and didn't soften in tempering zone either.
在试验的焊接条件下,WCX355超细晶钢在热影响粗晶区未有明显脆化,在回火区也未发生软化现象。
Under the experiment's welding condition, WCX355 ultrafine grained steels didn't distinctly embrittle in CGHAZ and didn't soften in tempering zone either.