其中以粉煤灰50%、硅灰10%取代普通硅酸盐水泥的试验组,无论是试验室标准养护或是加速老化试验都表现出最优的耐久性。
Among which the experiment group using 50% fly ash, 10% silica fume instead of ordinary Portland cement shows rather better durability either in standard curing or the accelerated aging experiment.