• 结果表明:经过喷雾干燥处理过的偏钨酸铵粉末颗粒呈球壳状,粉末体孔隙率高达71。

    The results show that the AMT powder with a special spherical shell structure exhibiting a high porosity of 71.

    youdao

  • 酸铵(AMT)原料采用喷雾干燥结合氢气还原方法成功制备出球形

    The spherical tungsten powder was fabricated by spray-drying method combined with hydrogen reduction using ammonium metatungstate (AMT) as raw materials.

    youdao

  • 酸铵(AMT)原料采用喷雾干燥结合氢气还原方法成功制备出球形

    The spherical tungsten powder was fabricated by spray-drying method combined with hydrogen reduction using ammonium metatungstate (AMT) as raw materials.