基于损伤理论,将用于评价体积型缺陷的APIRP 579公式进行了改进,建立了点腐蚀损伤管道的剩余强度评价公式。
Based on damage theory, residual strength assessment formula has been developed by modifying API RP 579 formula for volumetric flaw evaluation.
经过对32个实际焊接缺陷超声回波信号的分类识别,平面型缺陷的正确分类率为86%,体积型缺陷的正确分类率为78%;
The investigation of 32 natural weld defects show that 86% of the plane defects and 78% of the volume defects can be correctly classified.
而线缺陷型包裹体体积变化较大;
The inclusions trapped in line defect usually have different volumes.
点缺陷型包裹体体积一般较小,不方便分析;
Inclusions trapped in point defect mode are commonly in small size and not easy to be analyzed.
点缺陷型包裹体体积一般较小,不方便分析;
Inclusions trapped in point defect mode are commonly in small size and not easy to be analyzed.