以高铁酸钡为正极材料,二硼化钛为负极材料,碱性氢氧化钾溶液为电解质构成了一次性碱性电池。
Primary alkali battery was constituted with cathode of barium ferrate, anode of titanium diboride and KOH solution as electrolyte.