对含砷金矿石中的金的回收以往所采用的选(冶)矿工艺流程一般是浮选-氰化浸出和浮选-焙烧-氰化浸出工艺流程。
In general, the recovery of gold in arsenian gold ores usually is made by use of flotation cyanide leaching or flotation roasting cyanide leaching technological process.
依据矿物学特性,提出了“原矿浮选—精矿氧化焙烧— 氰化浸金—活性炭吸附金”的选冶联合工艺流程,金选冶总回收率达83.91%。
Based on the properties, a combined flowsheet of flotation-roasting in air -cyanidation-active carbon absorption was developed. The overall recovery of Au is of 83. 91%.
依据矿物学特性,提出了“原矿浮选—精矿氧化焙烧— 氰化浸金—活性炭吸附金”的选冶联合工艺流程,金选冶总回收率达83.91%。
Based on the properties, a combined flowsheet of flotation-roasting in air -cyanidation-active carbon absorption was developed. The overall recovery of Au is of 83. 91%.