• 采用此方法增韧环氧树脂贮存稳定性加热室温条件下固化,均能获得较高剪切强度T -剥离强度。

    The epoxy resin toughened by the above copolymer has excellent storage stability and, after cured by heating or at room temperature, it has higher shear strength and T-peeling strength.

    youdao

  • 通过使用本实验室设计低温拉伸夹具测定纳米二氧化硅改性环氧树脂复合材料室温液氮(77K)环境下的拉伸强度弹性模量和延伸率。

    Measurement of tensile strength , modulus and strain of nanometer SiO2/epoxy composite materials was conducted using self-designed tensile testing jigs at room temperature and 77K.

    youdao

  • 通过使用本实验室设计低温拉伸夹具测定纳米二氧化硅改性环氧树脂复合材料室温液氮(77K)环境下的拉伸强度弹性模量和延伸率。

    Measurement of tensile strength , modulus and strain of nanometer SiO2/epoxy composite materials was conducted using self-designed tensile testing jigs at room temperature and 77K.

    youdao