与重量法及容量法相比,采用火焰原子吸收分光光度法(AAS)测定天青石样品中的氧化锶含量,方法简单准确,干扰因素少。
Compared with weight method and volume method, determination of the contents of strontium oxide in Bluestone using AAS was more simple and accurate, and few factor disturbed the method.
以锆酸锶为基体,采用二氧化锆、巴德雷石粉和粒状聚苯乙烯为原料,制备了多孔陶瓷材料。
Porous ceramic materials on the base of strontium zirconate were developed with zirconium dioxide, baddeleyite powder, and granular polystyrol.
图片中呈现的效果通过使用氧化铜和碳酸锶实现。
In this case, copper oxide and strontium carbonate get the job done.
列维和他的同事们用原子力显微镜和两片绝缘体(镧氧化铝和锶钛氧化物),研制出了一枚纳米晶体管。
Using an atomic force microscope and two layers of insulators (lanthanum aluminum oxide and strontium titanium oxide), Levy and his colleagues created a nanoscale transistor.
用甘氨酸硝酸盐燃烧合成法,制备镧锶镍复合氧化物的陶瓷粉末。
A new combustion synthesis method, the glycine-nitrate process, has been used to prepare complex oxide ceramic powders of strontium-substituted lanthanum nickel.
用微等离子体氧化法在钛金属基体上制备钛酸锶钡(BST)陶瓷膜。
Barium strontium titanate (BST) ceramic film is prepared on titanium substrate by micro-plasma oxidation.
采用硝酸钴、硝酸锶及尿素为原料,通过溶胶-水热合成方法制备出掺锶钴氧化物前驱体。
By using cobalt nitrate, strontium nitrate and urea as initiative materials, the precursor of cobalt oxide was prepared by Sol-hydrothermal synthesis.
据实验条件下可溶性二氧化硅、锶溶出速率,估算出盘山地区偏硅酸型矿泉水的形成时间约为26年,锶型矿泉水形成时间约为8年。
Based on rate of SiO_2 and Sr in the test it is about 26 years to form slight Si-acidic mineral water and 8 years for Sr mineral water.
采用溶胶-凝胶法在硅基板上先分别制备钇稳定氧化锆(YSZ)和钛酸锶(STO)两种薄膜缓冲层。
The yttrium-stabilized zirconia(YSZ)and strontium titanium(STO)film buffer layers were prepared by Sol-gel process on Si substrates.
采用溶胶-凝胶法在硅基板上先分别制备钇稳定氧化锆(YSZ)和钛酸锶(STO)两种薄膜缓冲层。
The yttrium-stabilized zirconia(YSZ)and strontium titanium(STO)film buffer layers were prepared by Sol-gel process on Si substrates.