Moreover, the amorphous layer of 5 nm thickness in the initial stage provides nucleation sites for the groeth of c-axis oriented crystallites.
其中生长初期的约5nm左右的非晶层对形成c轴取向的AlN薄膜枝晶结构是有益处的。
参考来源 - 射频反应磁控溅射制备AIN薄膜及其物理性能分析·2,447,543篇论文数据,部分数据来源于NoteExpress
所制得的多层膜由一层单晶纳米片所组成的表面多孔层和一层或多层数目不等的底部非晶层组成。
The as-prepared film consists of a porous surface layer which was composed of many single crystal nanosheets, and one or more amorphous bottom layers.
研究激光形成非晶态的工艺条件与其表面硬度以及磨蚀及腐蚀的关系,并对非晶层的热稳定性进行测试。
The relationship was studied among the formation condition of the amorphous state and the surface hardness, abrasion and corrosion, and the heat endurance of the amorphous state was tested.
热浸镀铝-镧钢的扩散层中存在非晶态相,且稀土镧的添加可使扩散层中的非晶含量增加。
There is amorphous phase in diffusion layer of the hot-dip La-aluminizing and the content of the amorphous phase increases due to the addition of rare earths la.