本文主要介绍了中颗粒钨粉一步还原法的生产工艺及设备。
This paper has mainly described the one-step technical process and equipment for producing tungsten powder having medium particle size.
用液-固掺杂及两段还原法制备了氧化钪及铼掺杂的钨粉。
Scandia and rhenium doped tungsten powders were prepared by solid-liquid doping combined with two-step reduction method.
结果表明:还原温度是制取超细钨粉的关键因素,在适当的工艺条件下,可以使用蓝钨制得超细钨粉。
The results showed that reduction temperature is critical for the preparation of ultra-fine W-powder from blue tungsten oxide under appropriate technological conditions.