分析了T30S,Z30S两种切片及其纺丝拉伸等工艺对粗旦丙纶长丝不匀率的影响。
The effects of T30S and Z30S chips, spinning process and drawing process on yarn irregularity of coarse denier PP filament were analyzed.
纺丝过程中纤维皮层结构受到更大的拉伸取向作用,并在纤维表面出现一定游离原纤化结构。
A certain degree of free fibrillar structure was observed on the fiber surface due to the sheath structure of the fiber subjected to the greater drawing and orientation.
结果表明:随着磁粉含量的增加,磁性纤维的纺丝性能、拉伸性能、热性能下降。
The result showed that the spinning performance, drawing property and thermal property all decreased with the increase of magnetic particle content.