试验结果表明:在常温常压下,用硫酸浸出该氧化锌矿石锌的浸出率可达到78%。
It was found that 78% zinc extraction was obtained at room temperature and atmosphere pressure.
新工艺锌浸出率高,流程短,可在常温常压下浸出,无废液,具有较广阔的应用前景。
The new process has advantages of high zinc leaching rate, short flowsheet, leaching at normal temperature and pressure and no waste solution, suggesting a wide application field and good prospect.
试验表明,采用超声波强化浸出可使常温弱酸下不溶的铁酸锌浸出。
The results show that, with ultrasonic on the intensification of leaching, ZnFeO4, which do not be dissolved in weak acid leaching agent in normal temperature, will be leached.