silver coated glass bead 涂银玻璃珠
In short,according to lots of experiments,the best paste was containing 30%~35%F resin and 65%~70% silver-coated glass bead ,then the paste was cured at 140℃ for about 30 min.
综上所述,通过大量的实验研究发现,最佳性能的浆料是用F树脂30%~35%加入65%~70%的银包玻璃微珠粉调制浆料,然后在140℃下保温固化30min。
参考来源 - 新型低温聚合物导电浆料的制备及性能研究The effects of the addition level,particle size and modification technology of silver-coated glass bead and the curing degree of electrically conductive silicone rubber on the electrical conductivity of silver-coated glass bead/silicone rubber composite were investigated.
研究镀银玻璃微珠的用量、粒径、表面改性工艺以及导电硅橡胶硫化程度等对镀银玻璃微珠/硅橡胶复合材料导电性能的影响。
参考来源 - 镀银玻璃微珠/硅橡胶导电复合材料导电性能的影响因素·2,447,543篇论文数据,部分数据来源于NoteExpress
应用推荐