powder metallurgy superalloy 粉末冶金高温合金 ; 粉末高温合金 ; 粉末冶金高速钢
rene dt powder superalloy rene‘88dt粉末高温合金
nickel-based powder superalloy 镍基粉末高温合金
nickel-base powder metallurgy superalloy 镍基粉末冶金高温合金
superalloy powder 粉末高温合金
FGH95 superalloy powder FGH95高温合金粉末
base powder metallurgy superalloy 镍基粉末冶金高温合金
powder metallurgy nickel based superalloy 粉末冶金镍基高温合金
powder metallurgical superalloy 粉末冶金高温合金
CBN is an ideal tool material for finish and semi_finish turning powder superalloy. It not only ensures the high machining accuracy, but also can obtain longer tool life.
对精车和半精车而言,CBN是车削粉末高温合金的一种理想刀具材料,它不仅可保证高的加工精度,而且可获得长的刀具寿命。
By means of the measurement of creep curves and microstructure observation, an investigation has been made into the microstructure and creep behaviors of FGH95 powder nickel-base superalloy.
通过进行蠕变曲线测定和组织形貌观察,研究了FGH95粉末镍基合金的微观组织结构与蠕变行为。
An investigation of the surface of Ni-base superalloy powder particles in both as-atomized and as-HIP' ed conditions has been presented in the paper.
本文介绍了用扫描电子显微镜和俄歇电子谱仪观察和分析雾化态和热等静压态高温合金粉末颗粒的表面。