When the comparison was conducted between the 1000 h-time passage group and 6 months-time passage group,the most alter ofE* were occur in cadmium red and nanometre TiO2 coated with Si and Al with increasing amplitudes of 53.60%and 69.90% respectively.
对比避光保存的2组,前后色差差值最大的镉红组和硅铝包覆纳米TiO2组,避光保存6个月比1000 h色差分别增大了53.60%和69.90%。