The service life of screw steel wire rollers can be remarkably raised by using WC steel bonded carbide and suitable heat treatment technology.
用碳化钨钢结硬质合金制造螺纹钢丝轧辊,通过选用适当的合金牌号及热处理工艺,可显著提高轧辊的使用寿命。
Thermal fatigue crack forming process of steel bonded carbide containing 35% WC by the action of thermal stress has been observed time and time again.
对含有35 % WC的钢结硬质合金在热应力作用下热疲劳裂纹形成过程进行了反复观察。
WC steel-bonded cemented carbide powders being compacted by explosive compaction were bonded to the surface of carbon steel using liquid phase sintering.
采用液相烧结法将爆炸压实后的WC钢结硬质合金粉末复合在碳钢表面,对不同烧结温度下的界面组织和抗剪强度进行了研究。