Monel 400 mesh has low corrosion rate in flowing brackish or seawater while performing excellent resistance to stress-corrosion cracking in most freshwaters.
Monel 400目400目展品执行优异的耐应力腐蚀开裂最淡水而在流动的半咸水或海水的腐蚀速率低。
The results showed that 2091 alloy had better resistance to stress corrosion cracking than that of traditional 2024 (CZ) alloy.
并与传统的2024(CZ)合金进行了比较。 结果表明,2091合金具有较好的抗应力腐蚀能力。
So far, high-strength aluminum alloy has fairly high strength, but its stress corrosion cracking resistance needs to be further enhanced.
迄今,该系高强铝合金的强度已大幅提高,但抗应力腐蚀开裂性能有待改进。