K445 superalloy, as a kind of as-cast Nickel-based superalloy, has excellent combined properties. It is mainly used for the third and the forth grade blades of gas turbine engines.
K445高温合金是一种铸造镍基高温合金,具有良好的综合性能,其主要应用于燃气轮机的三、四级工作叶片。